TECHNICAL INFO
Technical Info
Corten Steel / Corrosion Resistant Steel Plates
Corten Steel
Weather resistant steel
Physical Properties
Chemical Properties
Chemical Composition (heat analysis, %)
In order to obtain fine grain structure a sufficient amount of nitrogen absorbing elements is added
(e.g. ≥0.02% Al).
Mechanical Properties, in the state of delivery condition.
At room temperature for plates ≥3mm in thickness (transverse test specimans, according to EN 10002). Requirements to hot rolled plates ≤3mm in thickness according to EN 10025-5.
*) 1 Mpa = 1N/mm2
The notched-bar impact energy is determined on ISO-V longitudinal test specimans at a temperature
of - 20°C as an average of three tests. For product thicknesses ≥10mm the average value is at least 27 J.
For thicknesses between 10mm and 6mm, the minimum impact value is reduced proportionally to the
speciman width (product thickness).
No impact test is performed on products below 6mm in thickness.
Number of Tests
*) as referenced in EN 10025-5
General Processing Information
Corrosion resistant steel - Weathering Steel grade
Corrosion Resistant Steel Plates
Weather resistant steel
Physical Properties
Weather resistant steel | Standard | Tensile Strength MPa | Yield Strength MPa | Elongation in 2 inches (min.) % |
Corten-A | US steel | 470-630 | 355 | 20 |
IRSM 41-97 | Indian Railways |
480 min | 340 min | 21 |
Chemical Properties
Weather resistant steel | C | Mn | P | S | Si | Cr | Ni | Mo | Cu | Fe |
Corten-A | 0.12 | 0.20-0.50 | 0.070-0.150 | 0.030 | 0.25-0.75 | 0.50-1.25 | 0.65 | - | 0.25-0.55 | - |
IRS M-41 | 0.10 | 0.25-0.45 | 0.075-0.112 | 0.030 | 0.28-0.72 | 0.35-0.49 | 0.20-0.49 | - | 0.30-0.39 | - |
Chemical Composition (heat analysis, %)
Grade | C | Si | Mn | P | S | Cr | Cu | V | Ni |
COR-TEN A | 0.12 | 0.25-0.75 | 0.20-0.50 | 0.07-0.15 | 0.030 | 0.50-1.25 | 0.25-0.55 |
|
0.65 |
COR-TEN B | 0.16 | 0.30-0.50 | 0.80-1.25 | 0.030 | 0.030 | 0.40-0.65 | 0.25-0.40 | 0.02-0.10 | 0.40 |
In order to obtain fine grain structure a sufficient amount of nitrogen absorbing elements is added
(e.g. ≥0.02% Al).
Mechanical Properties, in the state of delivery condition.
At room temperature for plates ≥3mm in thickness (transverse test specimans, according to EN 10002). Requirements to hot rolled plates ≤3mm in thickness according to EN 10025-5.
Grade | Minimum yield point (ReH Mpa *) |
Tensile strength Rm MPa |
Minimum elongation A (Lo=5.65 √So) % |
COR-TEN A |
355 | 470-630 | 20 |
*) 1 Mpa = 1N/mm2
The notched-bar impact energy is determined on ISO-V longitudinal test specimans at a temperature
of - 20°C as an average of three tests. For product thicknesses ≥10mm the average value is at least 27 J.
For thicknesses between 10mm and 6mm, the minimum impact value is reduced proportionally to the
speciman width (product thickness).
No impact test is performed on products below 6mm in thickness.
Number of Tests
1 tensile test | 1 test specimen per 40 t from each heat*) |
1 notched bar impact test | 1 set specimens per 40 t from each heat *) |
(3 specimens) | (at test temperature -20°C) |
*) as referenced in EN 10025-5
General Processing Information
Corrosion resistant steel - Weathering Steel grade
Corrosion Resistant Steel Plates
Atmospheric Corrosion Resistant Steel | |||
Steel Grade | Material No. | ||
TKS Standard | EN Standard | ASTM Standard | |
COR-TEN A | S355JOWP | ASTM A 242 TYPE 1 |
1.8946 |
Chemical Composition : |
||||||||||||||||
|
||||||||||||||||
Mechanical Properties : Hot Rolled Sheets |
||||||||||||||||
|
||||||||||||||||
Mechanical Properties : Cold Rolled Sheets = 3 mm in thickness |
||||||||||||||||
|